that it shines well.
730.
STUCCO FOR MOULDING.
Take of butter 6 parts, of wax 2 parts, and as much fine flour as when put with these 2 things melted, will make them as firm as wax or modelling clay.
GLUE.
Take mastic, distilled turpentine and white lead.
On bronze casting generally (731-740).
731.
TO CAST.
Tartar burnt and powdered with plaster and cast cause the plaster to hold together when it is